Layer overhang
At what overhang angle the bead loses support from the layer below.
The darker part rests on the layer below, the lighter part hangs in the air; the dot is the bead centre.
- Step-out
- 0.2 mm
- Supported share
- 56%
- Limit angle above it the centre hangs
- 48.4°
What you can see here
- For a wall to lean at from vertical, each layer steps out past the one below by ; at mm and 45° that is 0.2 mm.
- Only of the bead rests on the layer below: about 56% at mm and 45°. From (here 48°) its centre hangs, hence the rule of 45° without supports.
- A lower layer does not change the shape of the wall, because the step-out per millimetre of height is always . It splits it into finer steps and allows steeper overhangs.
- The angle is measured from vertical, as in Cura; PrusaSlicer measures from horizontal (30° here is 60° there). It is pure geometry: spreading plastic and cooling shift the limit in practice.
Formulas
- : step-out per layer (mm); : layer height (mm); : overhang angle from vertical
- supported part of the bead; : extrusion width (mm)
- the angle at which the bead centre stands over the edge of the layer below, that is